Results After 100 hours of artificial weathering, the one-way ANOVA result shows a highly significant increase in tensile and tear strengths with a minimal increase in hardness and roughness observed in samples containing 2% nanosilica (NS) followed by hybrid nanoparticle (HySA) of 1% nanoalumina (NA) + 1% nanosilica (NS) compared with a control group and other groups.
← all excerpts
Enhancement of Tech-Sil25 Maxillofacial Silicone Mechanical Properties after Artificial Weathering through Addition of Nanoparticles.