XRD data show that the (002) crystal face of 200 MPa zinc foil had an increasing trend, which is beneficial to the uniform and dense deposition of zinc ions (Fig.
← all excerpts
200 MPa cold isostatic pressing creates surface-microcracks in a Zn foil for scalable and long-life zinc anodes.