Figure 6 a shows the frictional curve at 400°C, COFs were decreased until 150 s, the COFs present an increasing trend between 150 s and 300 s, and then gradually stabilize.
← all excerpts
Preparation and tribological properties of multi-layer graphene/silicon dioxide composites-based solid lubricant coatings at elevated temperatures.