In Figure 4 a, a clear trend of variation in the component density can be seen, when the volumetric laser energy density gradually increased, while un-melted (I), semi-melted (II), melted (III), and over-melted (IV) cubes (10 × 10 × 10 mm 3 ) were formed.
← all excerpts
Process of Pure Copper Fabricated by Selective Laser Melting (SLM) Technology under Moderate Laser Power with Re-Melting Strategy.