It was proven by the quite significant increase in C-H bond intensity of the rHIPS samples at around 3000–2840 cm −1 after experiencing more reprocessing steps.
← all excerpts
From Electronic Waste to 3D-Printed Product, How Multiple Recycling Affects High-Impact Polystyrene (HIPS) Filament Performances.