However, when the strain-rate was 10 s −1 , the deformation zone formed by the matrix phase deformation was not as clear as the deformation zone formed when the strain-rates were 10 −3 s −1 and 1 s −1 and even showed a trend of layer-by-layer deformation, as shown in Figure 12 b.