What is worth noting is that the porosity shows a decreasing trend from 1300 °C to 1500 °C, from 56.3% to 47.1%.
← all excerpts
Impact of Sintering Temperature Variation on Porous Structure of Mo<sub>2</sub>TiAlC<sub>2</sub> Ceramics.
2
—
—
The sentences
With the increase in Ni content, the porosity showed a trend of first decreasing and then increasing, and the electrochemical active surface area (ECSA) of the electrode also showed the same changing trend.