The variation of hydrogen and heat production capacity showed a trend from high to low, i.e., 105.2 ± 9.7 mL/g and 1435.0 ± 30.3 J/g for the outer layer, 27.1 ± 4.4 mL/g and 80.4 ± 3.1 J/g for the inner layer, and 1.1 ± 0.01 mL/g and 1.2 ± 0.05 J/g for the middle layer.