In contrast, the ΔW values of MR/PET showed a trend of decreasing first and then increasing, reaching the minimum value of −8.23% and the maximum value of 4.19% at 416 and 490 °C, respectively.
← all excerpts
Thermal Behavior and Pyrolysis Kinetics of Mushroom Residue with the Introduction of Waste Plastics.
2
—
—
The sentences
In the first main stage, the weight losses of MR/PE-5:1, MR/PE-2:1, MR/PE-1:1, MR/PE-1:2, and MR/PE-1:5 were 29.16%, 9.63%, 14.13%, 6.20%, and 1.64%, respectively, which generally shows a decreasing trend with the increasing percentage of PE in the mixture (see Table 1 ).