The obtained results show a clear trend according to the pyrolysis temperature from ΔH q→0 = 31.8 kJ/mol for the W-500 sample to ΔH q→0 = 39.5 kJ/mol for the W-900 sample due to the increase of the microporosity of the biochar ( Table 2 ).
← all excerpts
Valorization of wipe wastes for the synthesis of microporous carbons and their application in CO<sub>2</sub> capture, gas separation and H<sub>2</sub>-storage.