3 E showed a clear trend of improving WVTR value for protein blended composite ENs (1,637 ± 22.24 - 2,142 ± 50.60 g/m 2 /d) relative to the pure PCL ENs (1,641 ± 50.65 g/m 2 /d).
← all excerpts
Unleashing the healing potential: Exploring next-generation regenerative protein nanoscaffolds for burn wound recovery.