Meanwhile, tensile strength showed a trend of increasing as the graphene percentage increased, compared to the PHA 89% 4HB copolymer, with a significant difference seen in the PHA 89% 4HB copolymer, between 6.5 MPa and 11 MPa, after the incorporation of bioactive glass and 0.1% of graphene.
← all excerpts
The Development and Characterisation of a P(3HB-<i>co</i>-4HB)-Bioactive Glass-Graphene Hydrogel as a Potential Formulation for Biomedical and Therapeutical Translation.