Additionally, a clear trend from 7–D to 21–D was observed, indicating that the coating pattern began with single-particle coating and gradually changed to a small aggregation (2–10 particles), finally reaching unevenly aggregated sedimentation.
← all excerpts
Functionalized Gold Nanoparticles for Facile Pattern-Controlled Surface Coatings.