Post fatigue, specimens showed a trend of increasing small and medium pore percentages, between 2,500 Image 9 and 25,000 Image 9 .
← all excerpts
Size effect characteristics and influences on fatigue behavior of laser powder bed fusion of thin wall GRCop-42 copper alloy.