The precipitation of α phase in the TC17-HAZ zone showed a trend of increasing and then decreasing, with the highest proportion of α phase after 740 °C annealing and reaching 75%.
← all excerpts
Effect of Preheating and Post-Heating on the Microstructures and Mechanical Properties of TC17-Ti<sub>2</sub>AlNb Joint with Electron Beam Welding.