Effect of Hydrothermal, Chemical, and Mechanical Degradation on Flexural Strength and Phase Transformation of Ground, Glazed, and Polished Zirconia.

Front Dent · 2024 · PMC11236485 · PMID 38993795

1
hedged sentence
closest p
boldest claim

The sentences

However, due to the small difference in the percentage of phases between the two groups, this difference did not reach statistical significance in our study.