Fineness, measured via an air permeability apparatus, was approximately 3600–4000 cm 2 /g and showed a trend of increasing as the limestone content increased.
← all excerpts
Optimal Limestone Content on Hydration Properties of Ordinary Portland Cement with 5% Ground Granulated Blast-Furnace Slag.