Accordingly, the compressive strengths of the geopolymers at 7 days and 28 days showed a trend of increasing and then decreasing when CaCl 2 was added.
← all excerpts
Effect of Calcium on the Setting Time and Mechanical Property of a Red Mud-Blast Furnace Slag-Based Geopolymer.