As the proportion of SDBS/MWCNTs increased from 0.26 to 0.34, the resistance value showed a trend of decreasing at first and then increasing.
← all excerpts
Structural Health Monitoring of Glass Fiber-Reinforced Polymer Laminates with Carbon Nanotube-Coated Glass Fiber Sensing Layer after Low-Velocity Impact Using Electrical Resistance Tomography.