Meanwhile, a substantially declined overall coefficient of 100 PPI cathode ( Figure S5B ), possibly due to the low neutron-attenuating elements such as C, O, and Si as hinted by the case of 100 PPI anode (bottom panels in Figure 8 ), showed a trend with notable changes along the thickness with a slight emphasis on the center ( Figure 7 F), similar to its volume profile.