Notably, in the last test where a plasticizer was used, the maximum accumulated temperature was reduced by approximately 19.3 °C, almost 30%, which is quite significant.
← all excerpts
New Methodology for Evaluating Strength Degradation from Temperature Increase in Concrete Hydration under Adiabatic Conditions.