The curve of MCS-6 showed a trend of increasing, then stabilizing, and then decreasing and was always higher than the curve of MC, which indicates that doping of 6% silt can effectively increase the unconfined compressive strength and resistance to dryness and wetness of sawdust.
← all excerpts
Strength Properties and Microscopic Experimental Study of Modified Sawdust Based on Solid Waste Synergistic Utilization.
2
—
—
The sentences
The strength profile of MCF-8 was consistently higher than the profile of MC after wet and dry cycling and lacked a decreasing trend, which was attributed to the more adequate hydration reaction of the 8% admixture of fly ash, echoing the findings of Nayak et al.