The UCS and tensile strength of the hardened slurries at 7 d and 14 d showed a trend of increasing and then decreasing as the proportion of BFS increased.
← all excerpts
Development and Application of Flue Gas Desulfurized Gypsum and Blast-Furnace-Slag-Based Grouting Material for Cracked Silty Mudstone.