3.5 Experimental Scattering Anisotropy Varies with Crystallinity and Counterion P-RSoXS data from undoped P3HT films reveals a clear trend: as the degree of crystallinity increases, so does the magnitude of scattering anisotropy up to the C 1s → σ* C – S transition at 287 eV, as illustrated in Figure 6 .