However, after reaching 110°C, an increasing trend in Ar-CH content was observed.
← all excerpts
Effects of pre-oxidation temperature and air volume on oxidation thermogravimetric and functional group change of lignite.
2
—
—
The sentences
Under 25mL/min and 50mL/min air volume conditions, the average activation energy of pre-oxidized coal samples in the high temperature oxidation stage showed a trend of first decreasing and then increasing with the increase of preset temperature conditions in the range of 40°C-110°C and 110°C-170°C.