a decreasing trendno p-value reported
As the content of graphene increases, the elongation at the break shows a decreasing trend, which is inferred to be caused by the uneven distribution of graphene.

also in 47,180 other papers

showed a trendno p-value reported
At the room temperature impact test, the impact strength showed a trend of increasing and then decreasing, and the maximum impact strength was 9.71 KJ/m 2 at a 2.0 wt% graphene content, which was 130.6% higher than that of PA6.