After the 12th cycle, the concentrations of Mo and As in the caustic leaching solution increased from 0.015 to 0.078 g/L and from 1.60 to 10.64 g/L, respectively. Si and P showed a trend of first increasing and then decreasing with an increasing number of cycles, with the decreasing trend starting after the seventh and third cycles, respectively.