Figure 3 above shows surface defects on samples printed with different laser powers.The size and number of the defects showed a quite significant reduction trend with the increasing of laser power to 340 W, and the defects became quite obvious with a further increasing of laser power to 420 w.
← all excerpts
A Study on the Electrochemical Performance of SLMed Al6061/TiB2 Composite Anodes Caused by Laser Power.