Although no statistically significant difference ( p > 0.05) was observed between the compressive modulus of the PLA 7.5%Mg group (2.79 ± 0.15 GPa) and that of the PLA 10%Mg group, the experimental data demonstrated a clear trend of enhanced mechanical properties in the composite scaffolds with increasing Mg content.