The wave velocity of the test blocks showed a trend of first decreasing and then increasing, and then it rapidly increased with an extension of the curing time.
← all excerpts
Study on the In-Laboratory Screening of Sandstone Grotto Patching Materials Based on Hydraulic Lime.