A clear trend is observed for M S values, increasing with cobalt loading, from 4.4 Am 2 kg −1 for 5.8%, to 8.3 Am 2 kg −1 for 9.2%, and to 26.1 Am 2 kg −1 for 13.3%, consistent with the increasing cobalt content estimated by XRF.