The results show a clear trend of increasing crosslinking density as the AAm content increases, ranging from 297 ± 5 mol/m 3 for 1.00:0.00 to 405 ± 12 mol/m 3 for 0.33:0.66 compositions.
← all excerpts
Engineering Thermo-Responsive Hydrogels with Tailored Mechanics for Biomedical Integration.