Specifically, the T g of IDE/LiTFSI_X/Y decreases to 23, 5, −7, and −19 °C, respectively, as the LiTFSI content increases, demonstrating a clear trend of reduced T g with higher LiTFSI composition.
← all excerpts
Mechanically Robust and Ion-Conductive Polyampholyte Elastomers via Dimeric Ionic Bonding.