For the binary system PVA/x Cu(TFSI) 2 , where “x” represents the weight ratio (WR) of Cu(TFSI) 2 to PVA, a clear trend was observed: the ionic conductivity (σ 1 ) escalated with increasing Cu(TFSI) 2 content, rising from 0.096 mS cm −1 for PVA to 1.012 mS cm −1 for PVA/60 wt% Cu(TFSI) 2 .