D iscussion In our study, the order of microhardness for micro-HA demonstrated a clear trend, with the highest values observed in the 5% concentration group, followed by 3 and 1%, and finally, RMGIC.
← all excerpts
Comparative Evaluation of the Effect of Incorporating Varying Percentages of Microhydroxyapatite on the Compressive Strength and Microhardness of Resin-modified Glass Ionomer Cement: An <i>In Vitro</i> Study.