From 5 to 30 wt %, EIS at 1.5 V in Figure e–h shows a clear trend that higher ionomer contents helped mitigate degradation in kinetic properties at the EOL (less changes in R ct ).
← all excerpts
Advancing the Performance of Anion Exchange Membrane Electrolysis by Employing a Powder-Based Ionomer during Anode Catalyst Layer Fabrication.
1
—
—