AKD–only samples show a clear trend of decreasing breathability compared to untreated CFM (105.58 cm 3 /cm 2 /s) with increasing AKD concentration.
← all excerpts
Sustainable, Safe, and Effective (Super)Hydrophobic Coatings for Cellulosic Fiber Material via Alkyl Ketene Dimer and Polysaccharide Integration.
2
—
—
The sentences
The AKD_alginate coating dispersions displayed a notable trend in surface tension, with the lowest value (48 mN/m) observed at the lowest AKD concentration.