Concurrently, the thickness of the passivation film exhibits a decreasing trend with increasing reduction ratio.
← all excerpts
Effect of Cold Rolling on the Mechanical Properties and Corrosion Resistance in Hydrofluoric Acid Solution of Inconel 600 Alloy.
2
—
—
The sentences
The experimental results ( Figure 6 , Figure 7 and Figure 8 ) demonstrate that with increasing cold rolling deformation, the number, diameter, and depth of pitting progressively increase, indicating a clear trend of localized corrosion intensification.