Barely Significant
← all excerpts

3D-Printed PLA/HA Composite Scaffolds: Balancing Mechanical Properties for Bone Tissue Engineering.

Materials (Basel) · 2026 · PMC13208693 · PMID 42195723

1
hedged sentence
0.5770
closest p · 11.5× alpha
0.5770
boldest claim

The sentences

did not reach statistical significancep = 0.577not close (p > 0.1)
Injection-molded pure PLA (PLA IM: 67.00 ± 0.56 MPa) exhibited compressive strength 23.2% higher than FDM-printed pure PLA (PLA FDM: 54.40 ± 0.64 MPa); however, this difference did not reach statistical significance after Bonferroni correction ( p = 0.577), reflecting the conservative nature of the correction at small sample sizes.

also in 111,027 other papers

Quoted from the open-access full text in Europe PMC under the licence the publisher applied. The sentence is reproduced exactly as published; the emphasis is ours.