The results reveal a clear trend: as the PS-g-AM concentration increases from 3% to 10%, the bitumen penetration value decreases noticeably, going from 62 dm for pure bitumen to 35 dm at 10wt% of PS-g-AM.
← all excerpts
Chemical grafting of waste polystyrene with acrylic acid and subsequent amine functionalization to enhance polystyrene modified bitumen characteristics.