8 a1–c1, before the initiation of crack propagation ( t − ti < 0 ) and after the initiation of crack propagation ( t − ti > 0 ), all samples display an increasing trend in the Mode-I SIF.
← all excerpts
Study on the dynamic failure performance of bamboo fiber/high-density polyethylene composites with different fiber content using digital image correlation.
3
—
—
The sentences
A clear trend emerges—as BF content increases, the crack propagation rate also increases (BPE8 > BPE5 > BPE2 > BPE0).
At 10-J impact energy, BPE samples with BF show a decreasing trend in crack propagation process as BF content increases, with BPE8 having the shortest crack propagation process at 16.6 mm.