First of all, as the amount of Li 2 MnO 3 increases, a clear trend is observed for the first oxidation peak at around 4 V which is probably due to the concurrent oxidations of Ni and Co.
← all excerpts
A Search for the Optimum Lithium Rich Layered Metal Oxide Cathode Material for Li-Ion Batteries.
1
—
—