( 21 ) indicated that MTA treated with saline had higher bond strength than the control MTA group; this finding was in contrast to our results since in our study, the push-out bond strength of the control group was higher than that of MTA treated with saline, but this difference did not reach statistical significance ( P >0.05).
← all excerpts
Effect of Smear Clear and Some Other Commonly Used Irrigants on dislodgement resistance of Mineral Trioxide Aggregate to Root Dentin.