To obtain a clear trend of the evolution of the three phases identified here as the discharge of sulfur-CuS hybrid electrode progresses, the peak area of three relatively strong reflections S (222), CuS (103), and Li 2 S (111) were chosen to be integrated at each depth of discharge and plotted together against discharge capacity in Fig. 2B .
← all excerpts
Operando Multi-modal Synchrotron Investigation for Structural and Chemical Evolution of Cupric Sulfide (CuS) Additive in Li-S battery.