A clear trend of gradually decreasing DTL was established with increasing temperature over the range of 23 to 140 °C for FFRP laminates following an impact energy of 5 joules, as seen in Figure 8 .
← all excerpts
Effect of Temperature and Water Absorption on Low-Velocity Impact Damage of Composites with Multi-Layer Structured Flax Fiber.