In the case of GAS 1 samples, the skin thickness does not show a clear trend with the part thickness, as instead observed for GAS 2.
← all excerpts
Lightweight High-Performance Polymer Composite for Automotive Applications.
2
—
—
The sentences
It is possible to note an increasing trend of the normalized modulus with the part thickness, until it reaches values close to 1 for the 4 mm thick samples.