For both cathodes, with the gradual increase of the current from 0.1 to 2 C (1 C = 1672 mA g –1 ), the specific capacity shows a clear trend of decrease.
← all excerpts
Cost-Effective Water-Soluble Poly(vinyl alcohol) as a Functional Binder for High-Sulfur-Loading Cathodes in Lithium-Sulfur Batteries.