Thus, whatever the parameter (force or energy) used to study adhesion, we observe a clear trend such as Adh G > Adh S2 > Adh S1 > Adh CML (Figs. 6 g, h), with little variations within the S2 layer, and therefore little dependence to the MFA.
← all excerpts
Influence of force volume indentation parameters and processing method in wood cell walls nanomechanical studies.