Despite these few missing values, there is a clear trend visible that “front horizontal” shows the lowest recovery properties, as already seen in the previous figures.
← all excerpts
Pressure Orientation-Dependent Recovery of 3D-Printed PLA Objects with Varying Infill Degree.
2
—
—
The sentences
On the other hand, a slight trend towards higher recovery properties for pressing on top in only visible for the quotient F 5 /F 1 , while for F 10 /F 1 , the measurement on top parallel to one of the edges shows slightly smaller values than those gained by pressing on the front diagonally or vertically.