It is easy to notice that when considering the samples with deformation coefficient λ equal to 1.33, the length of the elastic deformation region was estimated to be 4 times longer in comparison to the deformation coefficient λ equal to 1.1, which is experimental evidence that the extent of the elastic deformation region is fully related and dependable on the shape of the applied diameter reduction and die geometry, and the estimated differences were quite significant.
← all excerpts
Shape Analysis of the Elastic Deformation Region throughout the Axi-Symmetric Wire Drawing Process of ETP Grade Copper.